Textured surface of the paint film with uneven wave type formation. This happens when the surface of the paint film dries faster than the Cause substrate coats..
Common Cause
Excessive coat thickness.
Bad dry condition: ① too low or too high temperature. ② too large or too small air flow. ③
polluted air.
Insufficient flash-off time, or high temperature accelerated drying, or sun exposure.
Incorrect thinner: too powerful penetrability of thinner may swell to wrinkle.
Too long time for some synthetic resin baking finish to dry in the air before baking.
Sray polyurethane coat onto the existing nitryl paint and re-mend later.
Repair
(1) Make paint film completely dry.
(2) If slight affection, re-sand the affected area and polish.
(3) In serious case, remove the existing paint and apply the color system again.